Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 9.5 µm | 9.5 µm | median; Microtrac |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 9.5 µm | 9.5 µm | median; Microtrac |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 9.5 µm | 9.5 µm | mean aggregate size |
NanoScale NanoActive® Cerium Oxide NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the partic.. |
|||
Particle Size | 9.5 µm | 9.5 µm | median |
Esstech V-117-1095 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |