Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NanoScale NanoActive® Cerium Oxide

Category Ceramic , Oxide
Manufacturer NanoScale
Trade Name NanoActive®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoScale NanoActive® Cerium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the particle size.Applications: Applications include catalysts, enhancement of Near IR reflection, industrial coatings, polishing slurries, and reactive dopants.Information provided by NanoScaleComposition based on metal
Physical Properties Metric English Comments
Bulk Density 2.20 g/cc
0.0795 lb/in³
Density 6.00 g/cc
0.217 lb/in³
Loss On Ignition <= 5.0 %
<= 5.0 %
Particle Size 9.5 µm
9.5 µm
mean aggregate size
Specific Surface Area >= 50 m²/g
>= 50 m²/g
BET
Pore Size 0.00700 microns
0.000276 mil
Average Diameter
Component Elements Properties Metric English Comments
Cerium, Ce >= 99.7 %
>= 99.7 %
Processing Properties Metric English Comments
Moisture Content <= 3.0 %
<= 3.0 %
Descriptive Properties Value Comments
Appearance / Color Yellow Powder
Crystallite Size = 7 nm
Minimum Total Pore Volume cc/g 0.1
Users viewing this material also viewed the following: