Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning .. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app.. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast CURON 150 Dense Refractory Castable Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni.. |
|||
Particle Size | <= 7000 µm | <= 7000 µm | Grain Size |
Gouda Vuurvast CURON 150 H Dense Refractory Castable Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati.. |