Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 55 µm | 55 µm | median; Microtrac |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 55 - 65 µm | 55 - 65 µm | Mean |
Momentive Performance Materials PolarTherm® PTX60 Boron Nitride (BN) Powder Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic propert.. |
|||
Particle Size | 55 - 65 µm | 55 - 65 µm | 90% |
H.C. Starck Amperit® 140.1 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 55 - 63 µm | 55 - 63 µm | 90% |
H.C. Starck Amperit® 526.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 55 - 65 µm | 55 - 65 µm | 90% |
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 55 - 63 µm | 55 - 63 µm | 90% for WC-Co 83-17 |
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60) Composition is of NiSF RC 60 only |
|||
Particle Size | 55 - 63 µm | 55 - 63 µm | 90% |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | 55 - 75 µm | 55 - 75 µm | |
Lucite International Colacryl ® D80 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Particle Size | 55 - 75 µm | 55 - 75 µm | |
Lucite International Colacryl ® TS 1672 Acrylic Orthodontic Polymer A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai.. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline Aquasil® "BP" 2750 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline Dedusted Flake Series DF-2750 Aluminum Flake DF-2750 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with an uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dus.. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline SilBerCote® 2750-20Y SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts add.. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline SilBerCote® 2750-20Z SilBerCote® Z polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. Product is typically formula.. |
|||
Particle Size | 55 µm | 55 µm | Before Conversion |
Silberline Silvet® 760-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline Sparkle Silver® 2750 Sparkle Silver® 2750 is a coarse, regular purity , high sparkle, non-leafing aluminum pigment popular for solvent Automotive Applications. This pigment can be used with tints to produce a wide ra.. |
|||
Particle Size | 55 µm | 55 µm | Before Conversion |
Silberline Sparkle Silvet® 760-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline Sparkle Silvex® 760-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 55 µm | 55 µm | |
Silberline Sparkle Silvex® 760-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 55 µm | 55 µm | Before Conversion |
Silberline Sparkle Silvet® 760-20-E Sparkle Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compati.. |
|||
Particle Size | 55 µm | 55 µm | TEC QSD |
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | 55 µm | 55 µm | TEC QSD |
Trelleborg AEM Eccospheres® W-30 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | 55 µm | 55 µm | D50 |
ALM PA 605-A Filled Nylon 12 Prototyping Polymer 50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a.. |
|||
Particle Size | 55 µm | 55 µm | D50 |
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire.. |
|||
Particle Size | 55 µm | 55 µm | 50th% |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 55 µm | 55 µm | 50th% |
3M S15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 55 µm | 55 µm | D50 |
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe.. |
|||
Particle Size | 55 µm | 55 µm | Average D50; Laser Diffraction |
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer Information provided by Advanced Laser Materials (ALM). |
|||
Particle Size | 55 µm | 55 µm | Before Conversion |
Silberline Sparkle Silvet® 760-20-J Sparkle Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The pig.. |
|||
Particle Size | 55 - 63 µm | 55 - 63 µm | 90% |
H.C. Starck Amperit® 584.054 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
Particle Size | 55 - 73 µm | 55 - 73 µm | |
Lucite International Colacryl ® PD11SG Acrylic Dental Resin Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties... |