Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 50 µm | <= 50 µm | 90% smaller than |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
Particle Size | 50 µm | 50 µm | Average Diameter |
Potters Industries Conduct-O-Fil® AGSF-20 Silver-coated Hollow Ceramic Spheres Applications: Conductive paints and coatings; Aerospace and other mass-critical applications. Advantages include low density, easily mixed into paint systems, large particle sizeInformation provide.. |
|||
Particle Size | 50 µm | 50 µm | mean value |
Potters Industries Q-Cel® 6048 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 50 - 200 µm | 50 - 200 µm | spherical sizes available |
PPT FP110 Fully Sintered Ferrite Powder Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu.. |
|||
Particle Size | 50 - 200 µm | 50 - 200 µm | spherical sizes available |
PPT FP500 Fully Sintered Ferrite Powder Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu.. |
|||
Particle Size | 50 µm | 50 µm | D50; ISO 13320-1 |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Particle Size | 50 µm | 50 µm | Average; ISO 13320-1 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Particle Size | 50 - 85 µm | 50 - 85 µm | d50 |
Magyar Aluminum ALH-D80 Aluminum Hydroxide Wet type |
|||
Particle Size | 50 µm | 50 µm | D50 |
Malvern Minerals Wollastokup® FT Silane Treated Wollastonite Wollastokup® is a custom, silane treated calcium metasilicate (wollastonite) which is used as a functional filler in coatings, plastics, rubber and others due in part to its acicular or “too.. |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 105.074 Agglomerated Sintered Molybdenum (Mo) |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | |
Lucite International Colacryl ® TS2050 Acrylic Resin Lucite® Colacryl® TS2050 is a hard, methyl methacrylate based, acrylic resin with an especially tight particle size distribution, leading to extremely good performance in glass separation appl.. |
|||
Particle Size | 50 - 60 µm | 50 - 60 µm | 90% |
H.C. Starck Amperit® 140.3 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | >= 50 µm | >= 50 µm | |
Solvay Chemicals Rigmah® BO350 Information provided by Solvay |
|||
Particle Size | 50 µm | 50 µm | TEC QSD |
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | <= 50 µm | <= 50 µm | |
Epoxy Technology EPO-TEK® 430 Epoxy Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding .. |
|||
Particle Size | 50 - 80 µm | 50 - 80 µm | D(0.5) |
Akzo Nobel Expancel® 551 DE 80 d42 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 50 µm | 50 µm | Average D50; Laser Diffraction |
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer Information provided by Advanced Laser Materials (ALM). |
|||
Particle Size | 50 µm | 50 µm | D50 |
ALM PA-616-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.The PA 616-GS can be processed on any laser.. |
|||
Particle Size | 50 µm | 50 µm | D50 |
ALM PA-840-GSL Filled Nylon 12 Prototyping Polymer Engineered for excellent mechanical properties, part definition and surface finish.Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates .. |