Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 4.5 - 7.5 µm | 4.5 - 7.5 µm | average |
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 4.5 - 7.5 µm | 4.5 - 7.5 µm | average |
Malvern Minerals Novakup® Daper Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | <= 4.5 µm | <= 4.5 µm | 90% less than |
H.C. Starck Grade A Silicon Hexaboride, SiB6 |
|||
Particle Size | <= 4.5 µm | <= 4.5 µm | 90% less than |
H.C. Starck Grade F Titanium Diboride, TiB2 Powder for sintering.Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to.. |
|||
Particle Size | 4.5 - 7.0 µm | 4.5 - 7.0 µm | Laser Diffraction D50 |
H.C. Starck High Vacuum 250 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 4.5 - 7.0 µm | 4.5 - 7.0 µm | Laser Diffraction D50 |
H.C. Starck Standard 250 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | 4.5 µm | 4.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade AX 10 Silicon Metal Powder Si high purity min. 99.995%Raw material for reaction bonded silicon nitride (RBSN)Silicon metal infiltration for SiC (SiSiC) |
|||
Particle Size | 4.5 - 5.5 µm | 4.5 - 5.5 µm | D50 |
Solvay Luminostarâ„¢ Green A Phosphor Identification: Lanthanum Cerium Terbium Phosphate coprcipitateFormula: (LaxCeyTbz) PO4Main characteristics: Good homogeneity ensured by proprietary coprecipitation process, Stability and High react.. |
|||
Particle Size | 4.5 - 8.0 µm | 4.5 - 8.0 µm | d90, Guaranteed |
TIMCAL TIMREX® LSG6 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 4.5 µm | 4.5 µm | |
DayGlo Phantom IPO-15 Invisible Pigment, Orange These materials have a yellowish or white color body under visible light and produce a bright vibrant color when exposed to an Ultra-Violet light source. Phantom pigments can be used for security an.. |
|||
Particle Size | 4.5 µm | 4.5 µm | |
DayGlo Phantom IPO-18 Invisible Pigment, Green These materials have a yellowish or white color body under visible light and produce a bright vibrant color when exposed to an Ultra-Violet light source. Phantom pigments can be used for security an.. |
|||
Particle Size | 4.5 µm | 4.5 µm | Median |
CIMBAR CIMBAR™ CF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |