Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 10 µm | 10 µm | |
Poco Graphite PLS Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 410L Stainless Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals 4140/MA Low Alloy Steel Master Alloy Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52 % < 10 microns15% < 5 micronsMean size is 10.0 microns.Master alloy blended with 2 parts iron to.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals Fe50Cr Binary Alloy Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals H13 Tool Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals S2 Tool Steel Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals Cu10Al Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | 50% of particles |
Ferro CF 7567 Low-Temperature Sealing VITREOUS Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific therm.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro EG 0221 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro EG 0225 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | >= 10 µm | >= 10 µm | 20% finer |
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 10 µm | 10 µm | 87% finer than |
Imerys KT Cast Slurryâ„¢ Kaolin KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys |
|||
Particle Size | 10 µm | 10 µm | Average Particle Diameter |
Mitsui UNISTOLEâ„¢ R-100K Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Particle Size | 10 µm | 10 µm | Maximum of .1% less than |
H.C. Starck Amperit® 568.062 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35 Composition is of NiSF RC 60 only |
|||
Particle Size | 10 µm | 10 µm | maximum of 3% less than |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | <= 10 µm | <= 10 µm | SRRG Powder |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 10 µm | 10 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a.. |
|||
Particle Size | 10 µm | 10 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies MicroFLON® 1437 Thermoplastic Grade PTFE Additive Used in high temperature engineering plastics.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion... |
|||
Particle Size | 10 - 210 µm | 10 - 210 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Particle Size | 10 µm | 10 µm | |
Silberline EternaBrite® 601-1 EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborn.. |
|||
Particle Size | 10 µm | 10 µm | |
Silberline Sparkle Silver® 7005-AR Sparkle Silver® 7005-AR is a high quality, non-leafing, superfine pigment with exceptional whiteness and good flop effect. It is used mainly for its high hiding power (opacity) and distinctivenes.. |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG15C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | <= 10 µm | <= 10 µm | |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Particle Size | 10 - 16 µm | 10 - 16 µm | D(0.5) |
Akzo Nobel Expancel® 551 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 10 µm | 10 µm | 50" Percentile |
3M W-610 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | 10 µm | 10 µm | Median |
CIMBAR BARA 325 Barium Sulfate (BaSO4) BARA 200 is a natural, off-white barium sulfate. Cimbar's BARA 325 is a clean, high purity, high specific gravity, low solubility barium sulfate and it is chemically inert. These properties have m.. |
|||
Particle Size | 10 µm | 10 µm | |
Silberline StarBrite® 2180 These Vacuum Metallized Flake (VMF) pigments are extremely thin, non-leafing, lamellar aluminum pigments. These exacting characteristics allow the formulator to achieve a smooth, mirror-like metall.. |
|||
Particle Size | 10 µm | 10 µm | Mean |
Osprey Metals Co212-e Cobalt Alloy Powder (Grade 90% - 22) Particle size distribution 1-250 microns. Typical distribution:90% < 22 microns80% < 16 microns52% < 10 microns15% < 5 micronsMean size is 10.0 microns.SHAPE: Predominantly spherical PACKAGING:.. |