Information provided by China Tungsten
Physical Properties Metric English Comments
Bulk Density 2.60 g/cc
0.0939 lb/in³
Scott
Density 14.0 g/cc
0.506 lb/in³
Binder 2.0
2.0
wax
Particle Size 10 - 15 µm
10 - 15 µm
Mechanical Properties Metric English Comments
Hardness, Rockwell A 86
86
Tensile Strength, Ultimate 2700 MPa
392000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 15 %
15 %
WC 85 %
85 %
Descriptive Properties Value Comments
Flow Rate; sec/50g 31