Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 10 - 15 µm | 10 - 15 µm | d50 |
Magyar Aluminum ALOLT 8AF Aluminum Hydroxide Ground type |
|||
Particle Size | 7.0 - 15 µm | 7.0 - 15 µm | average |
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 7.0 - 15 µm | 7.0 - 15 µm | average |
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 11 - 15 µm | 11 - 15 µm | 10% |
H.C. Starck Amperit® 151.065 Tantalum (Ta) |
|||
Particle Size | 11 - 15 µm | 11 - 15 µm | 10% |
H.C. Starck Amperit® 161.065 Niobium (Nb) |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade A Silicon Hexaboride, SiB6 |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | 10% |
H.C. Starck Amperit® 140.3 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | 10% |
H.C. Starck Amperit® 146.3 Chromium (Cr) HS Number: 81122031 |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | d90, Guaranteed |
TIMCAL TIMREX® LSG10 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG13C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG15C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG6C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG11C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 10 - 15 µm | 10 - 15 µm | |
China Tungsten YG9C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 9.0 - 15 µm | 9.0 - 15 µm | D(0.5) |
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |