Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Akzo Nobel, Expancel
Trade Name Expancel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the thermoplastic shell softens and the gas increases its pressure, resulting in an expansion of the spheres.Applications: Anti-slip coatings; Braille paper; Carpet underlays; Printing ink
Physical Properties Metric English Comments
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Particle Size 9.0 - 15 µm
9.0 - 15 µm
D(0.5)
Thermal Properties Metric English Comments
Transformation Temperature 108 - 113 °C
226 - 235 °F
Expansion Starting Temperature
142 - 151 °C
288 - 304 °F
Temp at Max Expansion
Descriptive Properties Value Comments
Solvent Resistance 4
Scale of 1 to 5