Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 710 µm | 710 µm | Finer than |
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Particle Size | 710 µm | 710 µm | Finer than |
Inhance Fluoro-Seal INHANCE® HD-1035 HDPE Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to.. |
|||
Particle Size | <= 710 µm | <= 710 µm | 62%; Malvern |
SABIC Innovative Plastics NORYL SA120FIN PPE Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the.. |
|||
Particle Size | <= 710 µm | <= 710 µm | 0.62; Malvern |
SABIC Innovative Plastics NORYL SA120FIN PPE (Asia Pacific) Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the.. |
|||
Particle Size | <= 710 µm | <= 710 µm | 0.62; Malvern |
SABIC Innovative Plastics NORYL SA120FIN PPE (Europe-Africa-Middle East) Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the.. |
|||
Particle Size | 710 - 1000 µm | 710 - 1000 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-II Expandable Polystyrene (EPS) ONGROSTYR F-II is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |