Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 12 µm | >= 12 µm | 10% smaller than |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 12 µm | 12 µm | median; Microtrac |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 12 µm | 12 µm | Median Grain Diameter |
Nabaltec APYRAL® 16 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 17-7 PH Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | mean aggregate size |
NanoScale NanoActive® Magnesium Oxide Plus NanoActive MgO is produced using proprietary processes to obtain very high specific surface area (over 600 m2/g), small crystallite size, high porosity material possessing high chemical reactivity a.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 317L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 410L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 415 Low Alloy Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 430L Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 4365 Low Alloy Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Co212-e Cobalt Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Co452 Cobalt Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Co502 Cobalt Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals M2/MA Tool Steel Master Alloy Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Master alloy blended with 2 parts iron to produ.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Oxygen-Free Electronic Copper Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 - 16 µm | 12 - 16 µm | 90% finer than |
Potters Industries Sphericel® 110P8 Hollow Glass Spheres Description: Sphericel® 110P8 hollow glass spheres displace the same volume of resin as solid spheres of the same size, but are lighter. Using Sphericel® hollow glass spheres, plastics engineers c.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 17-4 PH Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Material Notes: Composition above is typical of.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 80/20 Ni Cr Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals Cu10Al Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |
|||
Particle Size | 12 - 18 µm | 12 - 18 µm | d50 |
Magyar Aluminum ALOLT 28AF Aluminum Hydroxide Ground type |
|||
Particle Size | 12 µm | 12 µm | mean |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Particle Size | 12 µm | 12 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline "L" Series L-270 L-270 is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This grade has a cornflake geometry and wide particle size distribution range. This grade can b.. |
|||
Particle Size | 12 µm | 12 µm | |
Shin-Etsu Silicones KSP-101 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 12 µm | 12 µm | |
Silberline Sparkle Silver® Premier 751 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Size | 12 µm | 12 µm | Typical |
TIMCAL TIMREX® PP 10 Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 12 µm | 12 µm | Average Crystal Size - Thin Section Test |
CoorsTek AD-94 Alumina (nom. 94% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 12 µm | 12 µm | 10th% |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 12 µm | 12 µm | Median Diameter |
Omya OMYACARB® 10 - AZ Calcium Carbonate A dry ground calcium carbonate with an intermediate and closely sized particle distribution.Applications: Am ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated.. |
|||
Particle Size | 12 µm | 12 µm | Mean |
Osprey Metals 440C Stainless Steel Powder (Grade 80% - 22) Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.SHAPE: Predominantly spherical PACKAGING: 4 &.. |