Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
NanoScale NanoActive® Cerium Oxide NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the partic.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
MarkeTech Repton EXP 93 Cordierite Mullite REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Bulk Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre.. |
|||
Bulk Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 60 S Moldable Refractory Material Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its.. |
|||
Bulk Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Bulk Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 50 D Moldable Refractory Material Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Sharadaa Ceramics HH 40D Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Sharadaa Ceramics HH 40SD Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Sharadaa Ceramics HH 42D Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Sharadaa Ceramics KYANITE HT Mullite Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Sharadaa Ceramics LI 50K High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF45 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.20 g/cc | >= 0.0795 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Du-Co Ceramics S-699 Alumina Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chosun Refractories AC-1 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chosun Refractories N1-2 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chosun Refractories N2-1 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chosun Refractories SF32 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chosun Refractories SF-S Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 2.20 g/cc | >= 0.0795 lb/in³ | |
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Bulk Density | 2.20 g/cc | 0.0795 lb/in³ | |
Chosun Refractories CRAG-L38 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |