Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | Tapped |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | Tapped |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | packed |
Imerys Minsparâ„¢ 4 Ground Feldspar Minsparâ„¢ 4 is a medium particle size, ground Feldspar with a tightly controlled particle size distribution. The small amount of material retained on a 325 mesh screen, in conjunction with excel.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Injection Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1895 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Loose |
Excalibar ExBar™ W 2 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® EXAD 3000 Polyvinylidene Fluoride - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Extrusion aid, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanic.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |