Polymer Property : Bulk Density = 0.0275 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.760 g/cc
0.0275 lb/in³
Loose
Nyco NYGLOS® M30 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 0.760 g/cc
0.0275 lb/in³
Loose
Nyco ULTRAFIBRE® M30 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 0.760 g/cc
0.0275 lb/in³
ASTM D4745
3M Dyneon™ CC607 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 35% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company
Bulk Density 0.760 g/cc
0.0275 lb/in³
ISO 60
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Bulk Density 0.760 g/cc
0.0275 lb/in³
ISO 60
FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound
BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial..
Bulk Density 0.760 g/cc
0.0275 lb/in³
Tap Density
SGL Carbon Group CF 3100 Graphite Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..