Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Loose |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir N 1840 Polystyrene General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir R 321P Polystyrene Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | |
Nabaltec APYRAL® 24 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Bulk Density | <= 0.650 g/cc | <= 0.0235 lb/in³ | |
Magyar Aluminum ALOLT 704 Aluminum Hydroxide Viscosity Optimized Type |
|||
Bulk Density | 0.650 - 0.850 g/cc | 0.0235 - 0.0307 lb/in³ | RP-0155 |
Solvay REPEL-O-TEX® SF2 Surfactant Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex SF2 has been specifically formulated for im.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 2482 Phenolic, Granular, Transfer Molded PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 4349 Phenolic, Granular, Compression Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 5482 Phenolic, Granular, Transfer Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 5488 Phenolic, Granular, Injection Molded PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Tap |
TIMCAL TIMREX® M150 mesh Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Powder Density; ISO 60 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 6301 Phenolic, Granular, Injection Molded PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i.. |
|||
Bulk Density | 0.650 - 0.800 g/cc | 0.0235 - 0.0289 lb/in³ | Powder Density; ISO 60 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | |
Daikin NEOFLON EC-6500 ETFE Coating Powder, White Description: 0.3-1.0 mm thickness.Processing Methods:Electro-static spray coating.Information provided by Daikin Industries. |
|||
Bulk Density | 0.650 - 0.800 g/cc | 0.0235 - 0.0289 lb/in³ | |
Addcomp ADD-VANCE® DS 485 Desiccant masterbatch in LLDPE carrier Fields of application: Highly concentrated desiccant masterbatch for LDPE, LLDPE, HDPE, PP, EVA and other ethylene copolymers.Examples: Elimination of moisture from (recycle) polymers in moisture se.. |
|||
Bulk Density | 0.650 - 0.800 g/cc | 0.0235 - 0.0289 lb/in³ | |
Addcomp ADD-VANCE® DS 785 Desiccant masterbatch in PP carrier Fields of application: Highly concentrated desiccant masterbatch for HDPE and PP.Examples: Elimination of moisture from (recycle) polymers in moisture sensitive applications.Mode of action and advan.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |
|||
Bulk Density | 0.650 - 0.850 g/cc | 0.0235 - 0.0307 lb/in³ | |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |