Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 35B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preforms for the "lost foam" casting technique used in foundries.Information provided by NO.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 45C Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from .. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 54B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product and reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, an.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 55B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fastmolding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Inform.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 55XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 64XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks f average and low densities.Information.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 65B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Production of average to high density blocks and molding of the shape of bulky packaging and parts for the building industry.Informat.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 76D Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. For the production of very low density blocks.Information provided by NOVA Chemicals. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | |
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin 19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EB6025 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Cosmetic packagingShower surroundsPoint of purchase displaysThin-wall injection molding and thermoformingFeatures:Smooth, glossy surface finishGo.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
NOVA Chemicals Gedexcel® 76L Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plates with low thermal conductivity.Information provided by NOVA Chemicals. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 3303 Phenolic, Granular, Injection Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 7507 Phenolic, Granular, Transfer Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EC6600 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Lithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Excellent printabilityMatte surface finishHigh hea.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons PUREX® LS 35 Carbon Black Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EA3025 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar.. |
|||
Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
Plenco 2311 Phenolic, Granular, Transfer Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |