Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | |
Oceanchem Group Melamine Cyanurate (MCA) Molecular Formula: C6H9N9O3Cas No.: 37640-57-6Physical Appearance: Fine, white, crystalline powder, nontoxic, odorless; indissolvable in water and most organic solvents.Use: Melamine Cyanurate is a .. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® HP 180 HP Carbon Black Specialty black designed for excellent dry grip as required for racing tiresHard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® HT™ P22PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® PEEK 150UF10 Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Magyar Aluminum ALO-P90-02 Alumina Alumina for Polishing |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Magyar Aluminum ALO-P95-01 Alumina Alumina for Polishing |
|||
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | ASTM D1895 |
LG Chemical PA1302 PVC General Description: PA1302, vinyl chloride copolymer with vinyl acetate exhibits excellent properties. It is easy to process and gives effective flow. Main Applications: Adhesive for sheet & film, .. |
|||
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | ASTM D1895 |
LG Chemical PB1752 PVC General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk.. |
|||
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | ASTM D1895 |
LG Chemical PB900 PVC General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary .. |
|||
Bulk Density | 0.300 - 1.60 g/cc | 0.0108 - 0.0578 lb/in³ | |
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ASTM D1895 |
Micropol DD Polyethylene powders for cleaning products Information provided by Micropol Limited |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-521 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-730 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-732 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-760 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-760G MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-870G MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
Zircar Ceramics ECO-1200B Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provid.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Dow Corning EP-9261 TI Cosmetic Powder This cosmetic powder provides smoothness and a powdery, non-greasy skin feel; high sebum absorption; soft focus; and improves SPF. As a white cross-linked dimethyl polysiloxane elastomer powder comb.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
BASF Paliotol™ Yellow K 1841 Color Additive Chemical Structure: Isoindoline YellowApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provide.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
BASF Theroplast® Black X70 Color Additive Application: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, PA and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Tap Density |
Momentive Performance Materials PolarTherm® PTX25 Boron Nitride (BN) Powder Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic propert.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® HP 160 HP Carbon Black Specialty black designed for excellent dry grip as required for racing tiresHard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKE™ RK-764 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKE™ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is endo.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Mil.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |