Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.280 g/cc | 0.0101 lb/in³ | ASTM D4895 |
3M Dyneon™ TF 9207 PTFE
(discontinued **) Low molecular weight virgin PTFEAgglomerate particlesEasily deagglomeratedInformation provided by Dyneon, A 3M Company |
|||
Bulk Density | 0.280 - 0.400 g/cc | 0.0101 - 0.0145 lb/in³ | ASTM D1895 |
LG Chemical LP170 PVC General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy.. |
|||
Bulk Density | 0.280 g/cc | 0.0101 lb/in³ | |
Zircar Ceramics AXL Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |