Physical Properties Metric English Comments
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 140 Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo..
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 145 CC Dense Refractory Castable
Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 150 H Dense Refractory Castable
Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati..
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable
Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan..
Bulk Density 1.60 - 2.20 g/cc
0.0578 - 0.0795 lb/in³
loose
Solvay Chemicals Barium carbonate granular
Barium carbonate granular is used for the production of display glass, crystal glass and other special glass, glazes, frits and enamels. Barium carbonate granular is also used in the chemical indust..
Bulk Density 1.60 - 2.20 g/cc
0.0578 - 0.0795 lb/in³
loose
Solvay Chemicals Strontium carbonate granular
Strontium carbonate granular is used in the production of display glass and other glass. Strontium carbonate granular is also used in the metallurgy.Information provided by Solvay