Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Barium carbonate granular

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Barium carbonate granular.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Barium carbonate granular is used for the production of display glass, crystal glass and other special glass, glazes, frits and enamels. Barium carbonate granular is also used in the chemical industry.Information provided by Solvay
Physical Properties Metric English Comments
Bulk Density 1.60 - 2.20 g/cc
0.0578 - 0.0795 lb/in³
loose
Descriptive Properties Value Comments
Composition <0.6%
S as SO3
>99%
BaCO3/SrCO3
Sieve Analysis <15%
<0.15 nm
0
>1.0 nm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved