Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.350 - 0.500 g/cc | 0.0126 - 0.0181 lb/in³ | |
Magyar Aluminum ALOLT 60DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.250 - 0.500 g/cc | 0.00903 - 0.0181 lb/in³ | |
Magyar Aluminum ALOLT 60F Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.350 - 0.500 g/cc | 0.0126 - 0.0181 lb/in³ | |
Magyar Aluminum ALOLT 60P Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Magyar Aluminum ALO-P90-02 Alumina Alumina for Polishing |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Magyar Aluminum ALO-P95-01 Alumina Alumina for Polishing |
|||
Bulk Density | 0.350 - 0.500 g/cc | 0.0126 - 0.0181 lb/in³ | |
Magyar Aluminum Zeolite |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1250 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1700 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.320 - 0.500 g/cc | 0.0116 - 0.0181 lb/in³ | |
Inhance Fluoro-Seal INHANCE® UH-1900 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH15 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH15C-10 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Metabolix Mirelâ„¢ I6003rp Biobased PHA Polymeric Modifier I6003rp PHA enhances the processing and properties of recycled PVC. Offering excellent inherent miscibility in PVC to enable improved processing, I6003rp can lower torque and improve flow, while imp.. |
|||
Bulk Density | 0.350 - 0.500 g/cc | 0.0126 - 0.0181 lb/in³ | |
Solvay Chemicals NOCOLOK® Cs Flux Flux for brazing magnesium aluminum alloysHS No.: 38109090/CAS-No.: 60304-36-1 and 138577-01-2Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Elect.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-521 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-730 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-732 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-760 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-760G MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-870 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-870G MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Dow Corning EP-9261 TI Cosmetic Powder This cosmetic powder provides smoothness and a powdery, non-greasy skin feel; high sebum absorption; soft focus; and improves SPF. As a white cross-linked dimethyl polysiloxane elastomer powder comb.. |
|||
Bulk Density | 0.400 - 0.500 g/cc | 0.0145 - 0.0181 lb/in³ | |
Addcomp ADD-VANCE® Cleaning Masterbatch Fields of application: Cleaning masterbatch for thermoplastic materials like olefins and styrenics. To be used in extruders and die-systems for all film- and filament / fibers lines as well as injec.. |
|||
Bulk Density | 0.420 - 0.500 g/cc | 0.0152 - 0.0181 lb/in³ | |
Akzo Nobel Expancel® 950 MB 120 Masterbatch with unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Bulk Density | 0.420 - 0.500 g/cc | 0.0152 - 0.0181 lb/in³ | |
Akzo Nobel Expancel® 950 MB 80 Masterbatch with unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKE™ RK-764 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKE™ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is endo.. |