Material Notes:
I6003rp PHA enhances the processing and properties of recycled PVC. Offering excellent inherent miscibility in PVC to enable improved processing, I6003rp can lower torque and improve flow, while improving PVC properties such as tensile toughness, hardness, and tear resistance. I6003rp is ideal for converters who want to increase their scrap usage rate without compromising quality, and for compounders who want to upgrade the value of their recycle PVC product range. Using I6003rp enables reformulation to reduce plasticizer, modifier, and stabilizer addition while maintaining physical properties.
Physical Properties Metric English Comments
Bulk Density 0.300 - 0.500 g/cc
0.0108 - 0.0181 lb/in³
Moisture Absorption at Equilibrium <= 0.35 %
<= 0.35 %
Metabolix STM-012
Viscosity Test 1.5 - 2.0 cm³/g
1.5 - 2.0 cm³/g
Intrinsic Viscosity; Metabolix STM-029
Crystallinity 20 - 60 %
20 - 60 %
Metabolix STM-003
Thermal Properties Metric English Comments
Melting Point 160 - 170 °C
320 - 338 °F
Metabolix STM-003
Glass Transition Temp, Tg -15.0 - 1.00 °C
5.00 - 33.8 °F
Metabolix STM-003
Optical Properties Metric English Comments
Yellow Index 35 - 45 %
35 - 45 %
ASTM E-313
Descriptive Properties Value Comments
Contamination 0 to 0.5 Particles/ Film
Metabolix STM-014 test
tc1/2 Crystallization 5 - 12 min.
Total Residual Solvent 67 to 250 ppm
Metabolix STM-005 test