Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid.. |
|||
Bulk Density | >= 2.75 g/cc | >= 0.0994 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | >= 2.75 g/cc | >= 0.0994 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | >= 2.75 g/cc | >= 0.0994 lb/in³ | Dried at 110°C |
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | >= 2.75 g/cc | >= 0.0994 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 007 Smart Cast Application Special Properties: Hot abrasion, Wear resistanceIndustry: SteelApplication: False Chute, Tundish BackupInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | >= 2.75 g/cc | >= 0.0994 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | 2.75 g/cc | 0.0994 lb/in³ | |
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | |
Chosun Refractories BATN-3 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | |
Chosun Refractories BATN-D2, Upper Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.75 g/cc | 0.0994 lb/in³ | |
Chosun Refractories CRAG-S81 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.75 - 2.81 g/cc | 0.0994 - 0.102 lb/in³ | |
Chosun Refractories CUN-718 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 2.75 g/cc | >= 0.0994 lb/in³ | |
China-Yixing Longly Refractories Plate Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Bulk Density | 2.75 g/cc | 0.0994 lb/in³ | |
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par.. |