Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.021 - 0.024 cm/cm @Time 86400 sec |
0.021 - 0.024 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 195 PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 195HP PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 215HPR PBT Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 295 PBT Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310HP PBT PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 311 PBT Unreinforced, improved resistance to UV. Medium viscosity. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 312 PBT Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific) Unreinforced, For compounding only (not for injection molding), Medium viscosity. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 325M PBT (Asia Pacific) 325M is a high flow VALOX 325 for restrictive gate tooling (key buttons)This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.024 cm/cm @Time 86400 sec |
0.019 - 0.024 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.024 cm/cm @Time 86400 sec |
0.019 - 0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.024 cm/cm @Time 86400 sec |
0.019 - 0.024 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.024 cm/cm @Time 86400 sec |
0.019 - 0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |