Coating Weight 13.4 g/m²
8.40 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 15MB400 OPP Film
Product Description: Bicor 15MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou..
Coating Weight 13.4 g/m²
8.40 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 15MB440 OPP Film
Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin ..
Coating Weight 13.4 g/m²
8.40 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 15MM288 OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. MM288 is designed for use as the center web of a triplex lamination. The treated surface offe..
Coating Weight 13.4 g/m²
8.40 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 15MM348 OPP Film
Product Description: An enhanced barrier metalized film with a very broad seal range and can be considered a multipurpose film. This designed of this film allow excellent performance on HFFS machine..