Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.875 - 2.24 g/cc
0.0316 - 0.0809 lb/in³
Average value: 1.11 g/cc Grade Count:307
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Density 0.970 - 2.24 g/cc
0.0350 - 0.0809 lb/in³
Average value: 1.32 g/cc Grade Count:46
Overview of materials for Silicone, RTV, Encapsulation Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value..
Density 2.18 - 2.24 g/cc
0.0788 - 0.0809 lb/in³
molded; ASTM D792
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide
PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne..
Density 2.22 - 2.24 g/cc
0.0802 - 0.0809 lb/in³
extruded; ASTM D792
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..