Physical Properties Metric English Comments
Density 2.05 - 2.15 g/cc
0.0741 - 0.0777 lb/in³
ASTM D792
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
Density 2.05 - 2.15 g/cc
0.0741 - 0.0777 lb/in³
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 2.00 - 2.15 g/cc
0.0723 - 0.0777 lb/in³
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 1.95 - 2.15 g/cc
0.0704 - 0.0777 lb/in³
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 2.10 - 2.15 g/cc
0.0759 - 0.0777 lb/in³
molded; ASTM D792
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite