Physical Properties Metric English Comments
Density 1.28 - 1.66 g/cc
0.0462 - 0.0600 lb/in³
Average value: 1.46 g/cc Grade Count:18
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Density 1.22 - 1.66 g/cc
0.0441 - 0.0600 lb/in³
Average value: 1.51 g/cc Grade Count:11
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Density 0.920 - 1.66 g/cc
0.0332 - 0.0600 lb/in³
Average value: 1.35 g/cc Grade Count:109
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Density 1.05 - 1.66 g/cc
0.0379 - 0.0600 lb/in³
Average value: 1.28 g/cc Grade Count:27
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Density 1.62 - 1.66 g/cc
0.0585 - 0.0600 lb/in³
ASTM D792