Physical Properties Metric English Comments
Density 0.890 - 1.21 g/cc
0.0322 - 0.0437 lb/in³
Average value: 1.06 g/cc Grade Count:130
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Density 0.923 - 1.21 g/cc
0.0333 - 0.0437 lb/in³
Average value: 0.944 g/cc Grade Count:94
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Density 1.16 - 1.21 g/cc
0.0420 - 0.0437 lb/in³
Lord Adhesives 17 Mix-In Accelerator for 200, 400, 500 Series
Lord Adhesives 17 Mix-In Accelerator for 200, 400, 500 SeriesLord Accelerator 17 mix-in accelerator for Lord 200, 400 and 500 series acrylic adhesives. Use at a 10:1 ratio.
Density 1.15 - 1.21 g/cc
0.0415 - 0.0437 lb/in³
Dow BETAMATE™ 1496 V Epoxy
BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle..
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 0145/R Flexible PVC, Injection Molding, Lead Free
Technical items with rubber/PU
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 58 Flexible PVC, Injection Molding for Footwear
Antislip soles
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 59/C Flexible PVC, Injection Molding for Footwear
Sandals
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 60/B Flexible PVC, Injection Molding for Footwear
Bicoloured soles
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 64/BT Flexible PVC, Injection Molding for Footwear
Soles for cold climates
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 65/T Flexible PVC, Injection Molding for Footwear
Crystal soles and sandals
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 650 Flexible PVC, Injection Molding for Footwear
Anti-slip soles
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds GS 66/BT Flexible PVC, Injection Molding for Footwear
Soles for cold climates
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Fainplast Compounds MPH 62 Medical Flexible PVC, Extrusion
Tubolar apparatus and peristaltic pump segments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Fainplast Compounds MPH 62/H Medical Flexible PVC, Extrusion
Technical tubes and peristaltic pump segments no DOP
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Fainplast Compounds MPH 62/OP Medical Flexible PVC, Extrusion
Tubolar apparatus and peristaltic pump segments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Fainplast Compounds MPH 63 Medical Flexible PVC, Extrusion
Tubolar apparatus
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Fainplast Compounds MPH 69/T Medical Flexible PVC, Extrusion
Technical tubes no DOP
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PG 60 Flexible PVC, Extrusion Modified with Rubber
Gaskets modified with rubber
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PH 60 Flexible PVC, Transparent Extrusion
Transparent profiles
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PH 66/A Flexible PVC, Transparent Extrusion
Profiles, UL Class V2
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PH 75/SN Flexible PVC, Transparent Extrusion
Transparent and flexible sheets
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PHS 60 Flexible PVC, Transparent Extrusion
Various profiles UV resistant
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PM 5010 Flexible PVC, Lead Free
Gaskets for frames
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PM 55/K Flexible PVC, Lead Free
Inner tube
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Fainplast Compounds KLT 79 Flexible PVC, Insulation Transparent Cables Lead Free
Transparent cables (90°C)
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
Average value: 1.20 g/cc Grade Count:74
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PG 62/K Flexible PVC, Extrusion Modified with Rubber
Gaskets modified with rubber opaque surface
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Fainplast Compounds PH 62 Flexible PVC, Transparent Extrusion
Transparent profiles
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO 1183
Austin Novel Materials Texalan® 785A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Density 0.951 - 1.21 g/cc
0.0344 - 0.0437 lb/in³
Average value: 1.03 g/cc Grade Count:22
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..