Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2060S (60105) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.960 - 0.964 g/cc | 0.0347 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2062T (62107) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.960 - 0.964 g/cc | 0.0347 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2062U (62111) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.960 - 0.964 g/cc | 0.0347 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2062x (62135) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2260M (601F7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.945 - 0.962 g/cc | 0.0341 - 0.0348 lb/in³ | Average value: 0.951 g/cc Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Density | 0.958 - 0.963 g/cc | 0.0346 - 0.0348 lb/in³ | |
Kazanorgsintez 276-288 High Density Polyethylene Composite Production Method: Compositions are achieved by gaseous-phase method. Application: Composition is intended for production of polymer film fibers contacting bulk food.Information Provided by Kaza.. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | |
Kazanorgsintez 294-73 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad.. |
|||
Density | 0.958 - 0.963 g/cc | 0.0346 - 0.0348 lb/in³ | |
Kazanorgsintez 295-73 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad.. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4960 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 8260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.956 - 0.962 g/cc | 0.0345 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HC 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.956 - 0.962 g/cc | 0.0345 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HC 7260 LS HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.956 - 0.962 g/cc | 0.0345 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HC 7260 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.960 - 0.962 g/cc | 0.0347 - 0.0348 lb/in³ | ASTM D792-00 |
Ipiranga Petrochem GP 100 BK HDPE The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Density | 0.959 - 0.963 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ DIUP Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 85507-79-5EC Number: 287-401-6Information provided by ExxonMobil |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ L911P Plasticizer Appearance: Clear and FreeAvailability: North AmericaCAS Number: 685151-43-5Information provided by ExxonMobil |