Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | ISO 845-88 |
Eurofoam Siliconcell 412/BT 130 Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | True, 3M QCM 14.24.6 |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | True, 3M QCM 14.24.6 |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.200 - 0.220 g/cc | 0.00723 - 0.00795 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic.. |
|||
Density | 0.200 - 0.220 g/cc | 0.00723 - 0.00795 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |