Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.96 g/cc | 0.360 lb/in³ | |
Indium Corp. Indalloy 145 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.97 g/cc | 0.360 lb/in³ | |
Indium Corp. Indalloy 48 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.97 g/cc | 0.360 lb/in³ | |
Indium Corp. Indalloy® 10 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Density | 9.96 g/cc | 0.360 lb/in³ | |
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into.. |
|||
Density | 9.96 g/cc | 0.360 lb/in³ | |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Density | 9.96 g/cc | 0.360 lb/in³ | |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Density | 9.96 g/cc | 0.360 lb/in³ | |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |
|||
Density | 9.96 g/cc | 0.360 lb/in³ | |
Lucas-Milhaupt Silvaloy® B72 Brazing Alloy Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may f.. |
|||
Density | 9.97 g/cc | 0.360 lb/in³ | |
Williams Advanced Alloys WS264 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |