Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.20 - 8.30 g/cc | 0.296 - 0.300 lb/in³ | |
Kennametal Stellite Denertiaâ„¢ N8 Nickel Dental Alloy Denertiaâ„¢ N8 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium free as defined by ISO 22674Information pr.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54 Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | P/M (98%) |
Kennametal Stellite Deloro® N-6 PM with P/M Processing Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing .. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 0% Cold Worked, Not Aged 0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes .. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 15% Cold Worked, Aged 15% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 25% Cold Worked, Aged 25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.75 inch (19.0 mm) o.d. and 0.065 inch (1.65 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.75 in.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 3.50 in.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.5 x 2.0 inch (13 x 51 mm) Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.5 x 2.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.62 in.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allvac® 718 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Jet engine rings, discs, shafts, compressor blades, seals, spacers. Fasteners, nuclear, oil & gas components. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 50% Cold Worked, Aged 50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Density | 8.19 g/cc | 0.296 lb/in³ | P/M (98%) |
Kennametal Stellite Deloro® N-6 PM cast Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing .. |
|||
Density | 8.20 g/cc | 0.296 lb/in³ | |
HP Alloys Alloy 718, 20% Cold Worked, Aged 20% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |