Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4567 Austenitic Stainless Steel Good corrosion resistance with excellent low cold work hardening properties.Applications: Suitable for manufacture of cold headed fasteners.Bar and rod forms. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
Indium Corp. Indalloy® 19 In-Bi-Sn Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Industeel URANUS® 65 310 L Modified Grade - Low C and Si for Nitric Acid Service Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric a.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Momentive Performance Materials Niobium Carbide (NbC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resist.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Goodfellow Iron 40/Nickel 38/Boron 18 Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 301 Austenitic Stainless Steel, Annealed Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 302 Austenitic Stainless Steel, 3/4 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 302 Austenitic Stainless Steel, Full Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 1/2 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 1/8 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel Description: S692/S693 MICROCLEAN are high-sulfur and low sulfur versions of high-carbon PM M4 high speed steel that is produced using state-of-the-art “Generation 3” powder processing technology... |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Carpenter AerMet® 100 Aged at 900°F An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high stren.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 0% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach Formadur® PH X Superclean Plastic Mold Steel Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steelCharacteristics: Excellent resistance to corrosion; Excellent polishability; Excel.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |