Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.50 g/cc | 0.271 lb/in³ | |
PSM Industries PolyAlloys MIM-14-4PH Heat Treated Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | |
PSM Industries PolyAlloys MIM-17-4PH sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | |
PSM Industries PolyAlloys MIM-430L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | |
PSM Industries PolyAlloys MIM-4605 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | |
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-30UH Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-35H Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-35SH Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-40H Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-40SH Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-42 Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-42SH Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-45 Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-45M Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-50 Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | |
BASF Sicopal® Yellow K 1160 FG Color Additive Chemical Structure: Bismut-vanadium oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA and PARecommendations for food applications: BgVV, FrancePhysical form.. |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-30EZ Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-33H Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-33SH Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-33UH Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-38M Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-40 Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-42H Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 - 7.80 g/cc | 0.271 - 0.282 lb/in³ | |
Alliance N-33M Neodymium Iron Boron Magnetic Material |
|||
Density | 7.50 g/cc | 0.271 lb/in³ | |
PSM Industries PolyAlloys MIM-430L sintered Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |