Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.651 - 2.930 g/cc | 0.09576 - 0.1058 lb/in³ | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Density | 2.651 - 2.930 g/cc | 0.09576 - 0.1058 lb/in³ | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Density | 2.651 - 2.930 g/cc | 0.09576 - 0.1058 lb/in³ | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Density | 2.651 - 2.930 g/cc | 0.09576 - 0.1058 lb/in³ | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Density | 2.651 - 2.930 g/cc | 0.09576 - 0.1058 lb/in³ | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |