Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Potters Industries Spheriglass® EMB-10 Low Alkaline Boro-Silicate Solid Glass Microspheres Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Potters Industries Spheriglass® EMB-20 Low Alkaline Boro-Silicate Solid Glass Microspheres Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Pyrotek Pinnacle Thermocouple Protection Tubes O'-Sialon (Bonded Silicon Carbide) TCPT The robust properties of Pinnacle Thermocouple Protection Tubes make it a superior alternative to competitive tubes in temperature measurement, maintenance and product life areas.ApplicationsCrucibl.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Ferro EG 2770 Specialty Glass Glass Type: Si-Al-Mg-Ca Typical Powder Form: TF Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Mateck Lithium Fluoride (LiF) Optical crystals |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Ferro EG 0002 Glazes and Sealants Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Ferro EG 3600 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott G018-093 Dental Glass Remarks: Sr- and F-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott GM31685 Dental Glass Remarks: Low refractive index glass ceramicApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCH.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott GM32087 Dental Glass Remarks: Sr-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
SGL Carbon Group EK 3235 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for .. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Density | 2.60 - 3.20 g/cc | 0.0939 - 0.116 lb/in³ | |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Zircar Ceramics HR-3M Dense Aluminum Oxide Support Rod ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | Fibre Density |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | Fibre Density |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber Information provided by HexCel |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | ASTM C20 |
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Du-Co Ceramics DC-9-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Corning Pyroceram® Glass Ceramic High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival ( pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. .. |
|||
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Density | 2.60 - 2.75 g/cc | 0.0939 - 0.0994 lb/in³ | |
3M Cool Roofing Granule (Wausau) 3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products are designed specifically to have a higher total solar reflectance than standard granules... |
|||
Density | 2.60 - 2.75 g/cc | 0.0939 - 0.0994 lb/in³ | |
3M Headlap Roofing Granule (Wausau) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott BG28 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |