Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Potters Industries Spheriglass® EMB-20 Low Alkaline Boro-Silicate Solid Glass Microspheres

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Spheriglass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Spheriglass® EMB-20 Low Alkaline Boro-Silicate Solid Glass Microspheres.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries.
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
Particle Size 10 µm
10 µm
Mean
2.0 - 20 µm
2.0 - 20 µm
Mechanical Properties Metric English Comments
Hardness, Mohs 6.5
6.5
Thermal Properties Metric English Comments
CTE, linear 5.10 µm/m-°C
2.83 µin/in-°F
Thermal Conductivity 1.03 W/m-K
7.16 BTU-in/hr-ft²-°F
Softening Point 830 °C
1530 °F
Optical Properties Metric English Comments
Refractive Index 1.53 - 1.57
1.53 - 1.57
Component Elements Properties Metric English Comments
Al2O3 14 %
14 %
B2O3 5.7 %
5.7 %
CaO 23.1 %
23.1 %
Fe2O3 0.20 %
0.20 %
K2O <= 0.50 %
<= 0.50 %
MgO 1.0 %
1.0 %
Na2O <= 0.50 %
<= 0.50 %
SiO2 55.5 %
55.5 %
Descriptive Properties Value Comments
Shape spherical