Physical Properties Metric English Comments
Density 2.56 g/cc
0.0925 lb/in³
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Density 2.56 g/cc
0.0925 lb/in³
LATI Latimass 62-07 D025 PA6, Impact Modified
Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Density 2.56 g/cc

@Temperature 25.0 °C
0.0925 lb/in³

@Temperature 77.0 °F
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Density 2.56 g/cc
0.0925 lb/in³
Schott ROBAX® Glass Ceramic
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s..
Density 2.56 g/cc
0.0925 lb/in³
ASTM C135
M Cubed Technologies RBBC-751 Reaction Bonded Boron Carbide
Reaction-bonded boron carbide for extreme wear environments. Can be cast into very large components (greater than 4 ft. square)Information provided by M Cubed Technologies, Inc.
Density 2.56 g/cc
0.0925 lb/in³
Fibre Density
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
Density 2.56 g/cc
0.0925 lb/in³
Schott BG3 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Density 2.56 g/cc
0.0925 lb/in³
Schott BG25 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Density 2.56 g/cc
0.0925 lb/in³
Schott BG26 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.