Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.56 g/cc
0.0925 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.70 µm/m-°C
<br>@Temperature -30.0 - 70.0 °C
4.83 µin/in-°F
<br>@Temperature -22.0 - 158 °F
10.1 µm/m-°C
<br>@Temperature 20.0 - 300 °C
5.61 µin/in-°F
<br>@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 487 °C
909 °F
Optical Properties Metric English Comments
Refractive Index 1.53
<br>@Wavelength 404.7 nm
1.53
<br>@Wavelength 404.7 nm
Hg
Transmission, Visible <= 1.0 %
<br>@Wavelength 540 - 680 nm
<= 1.0 %
<br>@Wavelength 540 - 680 nm
88 %
<br>@Wavelength 400 nm
88 %
<br>@Wavelength 400 nm
Internal transmittance of 96% at 400 nm
IR Transmittance 77 %
<br>@Wavelength 2500 - 2600 nm
77 %
<br>@Wavelength 2500 - 2600 nm
Internal transmittance of 84% from 2500-2600 nm.
UV Transmittance <= 1.0 %
<br>@Wavelength 200 - 300 nm
<= 1.0 %
<br>@Wavelength 200 - 300 nm
89 %
<br>@Wavelength 390 nm
89 %
<br>@Wavelength 390 nm
Internal transmittance of 97% at 390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0