Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series A-205 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0040 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 4MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series Glass Spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 5MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series Glass Spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0080 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 1.5MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 3MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries Ballotini® Impact Beads Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing. Coars.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Misumi Steatite MgO-SiO2Information provided by MISUMI Corporation. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres Appearance: Solid soda-lime glass beads with light green color in powder formTypical applications of GL0191 beads include: spacer material for gauge control, coating, filler for plastic, retroreflec.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0252 Blue Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with light blue color in powder form.Typical applications of GL-0252 glass microspheres include: spacer for gauge control, thermal expansion reduction .. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0262 Ni Coated Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with metallic nickel coatingTypical applications of GL-0262 glass microspheres include: conductive filler for plastic, pigment, and etc.Information pro.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres Appearance: Solid soda-lime glass microspheres with light green color in powder form.Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, fi.. |
|||
Density | 2.50 - 3.20 g/cc | 0.0903 - 0.116 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
Density | 2.50 g/cc @Temperature 25.0 °C |
0.0903 lb/in³ @Temperature 77.0 °F |
|
Schott ILLAX® Amber Pharmaceutical Glass Amber Glass Pharmaceutical primary packaging for oralia and solid dosageInformation provided by SCHOTT AG. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | Specification, After dried @ 110°C/24 hrs |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Schott G018-163 Dental Glass Remarks: Sr- and F-containing, very low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Pr.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Thermoseal KLINGER® top-chem-2000 PTFE Gasketing Fire Tested - API6FAUniversal application use in the chemical and petrochemical industriesFDA compatibleIdeal for higher temperatures and pressuresHolds shape for thermal cyclesPermits/Certification.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Du-Co Ceramics DC-10-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Ceradyne Ceralloy® 546 Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
AGY VeTron® Glass Fiber Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series A-120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series A-170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0060 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |