Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.71 g/cc | 0.0618 lb/in³ | |
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | |
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Quantum Composites QC-3450 48% Glass Fiber High Temperature Use SMC
(discontinued **) QC-3450 is highly reinforced with glass fibers. It is designed for compression molding of components requiring high structural strength and good resistance to elevated temperatures. Long-term use .. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Asia Pacific) LNP* Thermocomp* PF00C is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069S PA 66 LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 (Asia Pacific) LNP* Thermocomp* RFB66 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Covestro Baydur® STR/C-400 BB Polyurethane Composite SRIM Foam, 60% Glass Filled, MDI-based 2-Component Liquid System Contains directed chopped fiber preform glass.0.16 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bay.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-61 Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Conditioned, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.71 - 1.78 g/cc | 0.0618 - 0.0643 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |
|||
Density | 1.71 g/cc @Temperature 23.0 °C |
0.0618 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT 403 M-G50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Density | 1.71 g/cc @Temperature 25.0 °C |
0.0618 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Plaslok 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 501 is a two-stage, mineral and flock.. |