Density 1.206 g/cc
0.04357 lb/in³
ISO 1183
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber
PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance
Density 1.206 g/cc
0.04357 lb/in³
ISO 1183
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified
Density 1.206 g/cc

@Temperature 140 °C
0.04357 lb/in³

@Temperature 284 °F