Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.10 g/cc | 0.0397 lb/in³ | Relative, no post cure- press cured for 5 minutes; ASTM D792 |
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.10 - 3.80 g/cc | 0.0397 - 0.137 lb/in³ | Average value: 1.49 g/cc Grade Count:605 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Density | 1.10 - 1.14 g/cc @Temperature 300 - 300 °C |
0.0397 - 0.0412 lb/in³ @Temperature 572 - 572 °F |
Average value: 1.11 g/cc Grade Count:3 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | uncured |
Permabond UV630 UV-curable Adhesive PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Techmer ES Electrafil® DB-1200/SS/4 ABS, 4% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 LX Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Silon TA 2343 HD Black Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD, TA 1116 HD and TA 1117 HD.TA 2343 HD, together with the above mentioned graft, contains the cross-linking catalyst to.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Suzhou Hipro Polymers Hiprolon® 211 PES Colorized Nylon powder Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Tipco Tipcolene® UV 1006 - Combination of UV Stabilizer & UV Absorber Masterbatch with 15% UV & Anti-Oxidants in LDPE |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183-87 |
Wellman Wellamid® XT1606-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Loctite® 4471 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
DSM Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance... |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0437G30CL Glass Reinforced Coupled |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Tipco Tipcolene® HR 7224 - 25% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer 25% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 1.10 - 1.14 g/cc | 0.0397 - 0.0412 lb/in³ | Average value: 1.13 g/cc Grade Count:28 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Polyram RamLloy A001 Nylon 66/Polyethylene Alloy for Injection Molding, Impact Modified Nylon 66/PE Alloy, reduction of water absorption, impact modified, for injection molding applications.Information provided by Polyram. |