Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | <= 0.950 g/cc | <= 0.0343 lb/in³ | ISO 1183 |
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Density | 0.950 - 0.954 g/cc | 0.0343 - 0.0345 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.950 - 0.954 g/cc | 0.0343 - 0.0345 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6753G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE
(discontinued **) Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes.. |
|||
Density | 0.949 - 0.955 g/cc | 0.0343 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GP 9452 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Density | 0.949 - 0.955 g/cc | 0.0343 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 9450 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® FB 29 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total 1285 HDPE film Applications: T-shirt sacks, trash can liners, merchandise bags, coex applicationsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total 49080 UV HDPE blow molding FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E924 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Covestro Bayflex® 110 RIM-LITE Polyurethane Elastomeric RIM, 13% Mineral Filled, MDI-based 2-Component Liquid System Contains 10% calcium silicate and 3% glass microspheres.0.15 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183/A |
ExxonMobil Exxtral™ BMV 102W Performance Polyolefin Product Description: Polyolefin injection molding compound with high flow, good low-temperature impact resistance, and excellent processability for painted, partial painted, and molded-in-color auto.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti.. |
|||
Density | 0.949 g/cc | 0.0343 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Density | 0.950 g/cc @Temperature 23.0 °C |
0.0343 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate LOTRYL® 28 MA 07 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 28 MA 07 is a polyme.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Aclo Accucomp Polyethylene HD0200L High Density |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Buckeye Polymers BP RPPC 0510 Blk Reprocessed Polypropylene, Unfilled This reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds are utilize.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
BASF N4-Amine S N,N'-Bis-(3-Aminopropyl)ethylene-diamine Formula: C8H22N4CAS: 10563-26-5Description: N4-Amine S is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 1,3-Propanediamine,N,N”-1,2-ethanediylbis- 1,5,8,1.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
BASF Neodecanoyl Chloride Formula: C10H19ClOCAS: 40292-82-8Description: Neodecanoyl chloride is a colorless liquid, with a pungent odor. It is also miscible with water.Synonyms: Neodecanoic acid chlorideApplications: Interm.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | TPE-0105 (ASTM D792) |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Density | 0.950 - 1.20 g/cc | 0.0343 - 0.0434 lb/in³ | Average value: 1.13 g/cc Grade Count:94 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |