Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D 792 |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ISO 1183 |
DSM Yparex® 8104 R Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Eastman 808P Polyethylene
(discontinued **) Low density polyethylene 808P is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of .. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Global SU-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
LyondellBasell Montell 0300 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
Density | 0.917 g/cc @Temperature 20.0 °C |
0.0331 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PM Propylene glycol methyl ether Available in electronic grade.Information provided by Lyondell. |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-278 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | |
LyondellBasell Lupolen® 1800 S LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake EM1550AA Low Density Polyethylene WESTLAKE low-density polyethylene EM1550 is a low-density formulation used for injection molding applications.Application/UsesFlexible medicalLidsMedicalFDA: This material complies with FDA regulati.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake EM811AA Low Density Polyethylene WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.Application/UsesFlexible medicalMedicalFDA: This .. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake Hifor Xtreme SC74842 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74842 polymer is a high strength and good clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. Films produced wit.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LD 200.48 Extrusion Coating and Laminating Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 251 Low Density Polyethylene Resin (European Grade) Product Description: LD 251 is an LDPE extrusion coating grade, offering:low neck-in excellent heat sealablity (ie high seal speeds and/or seal temperatures mostly required in high speed form-fill a.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2267G Linear Low Density Polyethylene A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | |
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D-1505 |
Bapolene® 142B Polyethylene Film Grade Bapolene 142B is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 900 Low Density Polyethylene IPETHENE® 900 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high melt flow rate, good transparency, and flexibility. .. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LD 206.48 Extrusion Coating Resin
(discontinued **) LD 206.48 is a extrusion coating grade, having good organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers.Information provided by ExxonMobil Chemic.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |