Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | Average value: 0.903 g/cc Grade Count:89 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8249 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Sheet extrusion; Thermoforming; Extrusion, injection, stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlComplies with FDA specific.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Innovene 1088 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: General purposeTypical applications: Water quenched blown filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3119HS Ultra High Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High stiffness, Low Temperature impactComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.886 g/cc @Temperature 15.6 °C |
0.0320 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 150 ND Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | |
Dow AFFINITY™ SM 8250 Polyolefin Plastomer AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flex.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | |
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Density | 0.887 g/cc | 0.0320 lb/in³ | |
ConocoPhillips Hydroclear® 220 5 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | |
BASF NEOL® Neolpentylglycol Pure Liquid Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) pure liquid is a colorless melt, with a sweetish odor. Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dim.. |
|||
Density | 0.885 g/cc @Temperature 23.0 °C |
0.0320 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18390 Maleic Anhydride Modified Polyethylene OREVAC® 18390 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H08U-00 Polypropylene Homopolymer, Fiber Grade Suggested fabrication methods: Fiber spinningFeatures: UV stable, High tenacityTypical applications: Geotextiles, Continuous filamentComplies with FDA specification, Title 21, CFR 177.1520.Typical p.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 6219 Homopolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Sheet extrusion; ThermoformingFeatures: High clarity, High heat resistance, Good melt strength/flow balanceTypical applications: Rigid packagingComplies with FDA speci.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7635 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H07D-00 Polypropylene Homopolymer Grade H07D-00 is a polypropylene homopolymer for cast film applications that require slip and antiblock additives. This resin meets the requirements of the Food and Drug Administration as specified .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8449 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlTypical applications: Housewares, Rigid packagingComplies wit.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8649X Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Developmental Grade. Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Low taste/odor, Excellent processabilityTypical applications: High clarity c.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9117 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Sheet; ExtrusionFeatures: Improved MVTR, Stain resistanceTypical applications: Film, Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical pro.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |