Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.880 - 1.62 g/cc | 0.0318 - 0.0585 lb/in³ | Average value: 1.34 g/cc Grade Count:85 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® 3885 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® 4675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT315 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT485 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT515 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT521 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ISO 1183 |
Polyram Bondyram® 7103 Maleic Anhydride Modified Ethylene-Alpha Olefin Copolymer High flow impact modified for Nylon compounds un-reinforced and glass fiber reinforced. Good retention of impact at low temperatures.Information provided by Polyram. |
|||
Density | 0.880 g/cc @Temperature 15.0 °C |
0.0318 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Heavy Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.879 g/cc @Temperature 15.0 °C |
0.0318 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Rarus 427 The Mobil Rarus 400 Series is a line of premium performance ashless air compressor lubricants designed to meet the stringent requirements of the major compressor manufacturers. They are formulated w.. |
|||
Density | 0.880 g/cc @Temperature 15.0 °C |
0.0318 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Solvesso™ 100 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.880 g/cc @Temperature 15.0 °C |
0.0318 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 15W-40 Exxon XD-3 Extra Exxon XD-3 Extra 15W-40 is a premium, heavy duty diesel engine oil that provides outstanding protection to modern, high performance engines used in the toughest on and off highway applications. Exxo.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |
|||
Density | 0.880 g/cc @Temperature 15.6 °C |
0.0318 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Mobil Pegasus 15W-40 40 Mobil Pegasus Special is a high quality SAE 15W-40 gas engine oil primarily intended for the lubrication of crankcases and power cylinders of spark-ignited two- and four-cycle gas-fueled engines. It.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
ConocoPhillips Hydroclear® 100 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |
|||
Density | 0.880 - 0.920 g/cc | 0.0318 - 0.0332 lb/in³ | RP-17617 |
Solvay RHODOLINE® 670 Surfactant Description: Highly effective mineral oil defoamer for latex processing..Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE 670 is an APE-free and silicone–free def.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
3M 230 Crystal Clear Sealant 3M™ Crystal Clear Sealant 230 is a one component thermoplastic elastomer which forms permanent elastic bonds when used in surface sealing applications. 3M Crystal Clear Sealant 230 bonds to a wide .. |