Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D792 |
Protective Coating PC-Woody® Epoxy Paste PC-WOODY® is an epoxy paste formulated to replace missing and rotted wood with structural strength greater than most wood. Use for permanent repairs on all types of wood-exterior or interior. Unl.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | Dry |
Unifrax Fiberfrax® LDS AL-Moldable Moldable Insulation Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b.. |
|||
Density | 0.720 g/cc | 0.0260 lb/in³ | |
Zircar Ceramics HASH-60 Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type HASH-60 is a hardened insulation board used primarily for its high temperature dielectric strength in high power electrical switching equipment. Inform.. |
|||
Density | 0.720 g/cc | 0.0260 lb/in³ | |
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.720 g/cc | 0.0260 lb/in³ | |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Density | 0.720 g/cc | 0.0260 lb/in³ | |
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastic.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | ASTM C134 |
BNZ Materials BNZ-25 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.719 g/cc | 0.0260 lb/in³ | |
3M Foam Fast 74 Spray Adhesive An extremely fast tacking industrial grade spry adhesive for bonding foam and fabricFeatures:Used for bonding flexible urethane or latex foam together and to other materials such as wood, metal and .. |
|||
Density | 0.719 g/cc | 0.0260 lb/in³ | |
3M Hi-Strength 90 Spray Adhesive An industrial grade spray adhesive that is typically used for bonding HPL to woodFeatures:A high strength, fast, contact-type adhesiveExcellent adhesive for decorative laminates, particleboard, and .. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | ASTM D1056 |
ACC Magnifoam™ MFSILTEC™-HD MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Density | 0.719 g/cc | 0.0260 lb/in³ | |
3M Super 77™ Multipurpose Spray Adhesive A high tack, high coverage and fast drying adhesiveFeatures:A high tack, high coverage fast drying, transparent adhesive for permanently attaching foils, carpeting, many lightweight foams, permanent.. |
|||
Density | 0.719 g/cc | 0.0260 lb/in³ | |
3M Scotch-Weld™ Foam Fast 74 Cylinder Spray Adhesive An extremely fast tacking industrial grade spry adhesive for bonding foam and fabricFeatures:Used for bonding flexible urethane or latex foam together and to other materials such as wood, metal and .. |
|||
Density | >= 0.721 g/cc | >= 0.0260 lb/in³ | |
Monmouth Rubber & Plastics Superbounce 90 NEO/SBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.720 g/cc | 0.0260 lb/in³ | |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
Pyrotek Wollite 45 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Density | 0.720 g/cc | 0.0260 lb/in³ | |
BASF N,N-Dimethylisopropylamine Formula: C5H13NCAS: 996-35-0Description: Dimethylisopropanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: Dimethylisopropanolamine, 1-Dimethylamin.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
BNZ Materials 2645LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |